Equipment / Precision Wafering

PICO-200S Manual Table Feed Precision Wafering Saw

The PICO-200S Manual Precision Saw is ideal for metallographic cutting of small samples. With adjustable speeds (500–3000 rpm), support for 6–8" blades, and manual control, it ensures precision and versatility. Features include immersion cooling, speed display, and dual vises—all in a compact, durable design.

Technical Specifications - PICO-200S

Parameter Specification
Cut-off Blade Size Max. diameter 200 mm (8 inches)
Cutting Capacity 30 mm (1-inch)
Specimen Feed Table feed
Coolant Tank 3 Liters
Arbor Size 12.7 mm (0.5 inches)
Variable Speed (RPM) 500-3000 rpm continuously adjustable with electronic speed display
Motor Power 400 W
Electrical Specification 110V/220V (50/60 Hz)
Dimensions (WxDxH) Hood closed: 18.5 x 20 x 14-inch (47 x 50.5 x 36 cm) / Hood open: 18.5 x 22 x 25-inch (47 x 56 x 63 cm)
Weight 45 kg (100 lbs)
Catalog Number PICO-200S