Microhardness Testers

Microhardness Testers

Microhardness Testers from PACE Technologies deliver precision and reliability for evaluating the hardness of thin films, coatings, and microstructures in metallographic applications. Engineered for accuracy and consistency, these testers offer versatile testing capabilities with Vickers and Knoop methods, making them ideal for both routine quality control and advanced research environments. With our range of microhardness testers, you can ensure detailed analysis and compliance with industry standards.

ALPHA-MHT-1000Z Digital Microhardness Tester

Technical Specifications - ALPHA-MHT-1000Z

Parameter Specification
Test Force Range 10gf to 1000gf
Optical Magnification 100X, 400X (10X and 40X objectives)
Auto Turret Included
Dwell Time Adjustable 5-60 seconds
Resolution 0.1µm
Construction Aluminum and stainless steel
Dimensions (WxDxH) 12.8 x 19 x 21.5 inches (325 x 480 x 545 mm)
Weight 68 lbs (31 kg)
Part Number ALPHA-MHT-1000Z


ALPHA-MHT-2000Z2 Touchscreen Microhardness Tester

Technical Specifications - ALPHA-MHT-2000Z2

Parameter Specification
Test Force Range 10gf to 2000gf
Optical Magnification 100X, 400X (10X and 40X objectives)
Digital Display Touchscreen
Dwell Time Adjustable 5-60 seconds
Auto Hardness Conversion HRA, HRB, HV
Construction Aluminum and stainless steel
Maximum Sample Height 3.5-inches (90 mm)
Dimensions (WxDxH) 12.8 x 19 x 21.5-inch (325 x 480 x 545 mm)
Weight 70 lbs (32 kg)
Part Number ALPHA-MHT-2000Z2


ALPHA-MHT-AUTO Automated Microhardness Tester

Technical Specifications - ALPHA-MHT-AUTO

Parameter Specification
Test Force Range 10gf to 1000gf
Optical Magnification 100X, 400X (10X and 40X objectives)
Automation Fully Automated
Dwell Time Adjustable 5-60 seconds
Resolution 0.1µm
Construction Aluminum and stainless steel
Maximum Sample Height 6.7 inches (170 mm)
Dimensions (WxDxH) 13.2 x 22 x 26.6-inch (335 x 560 x 675 mm)
Weight 115 lbs (52 kg)
Part Number ALPHA-MHT-AUTO


ALPHA-MHT-1000VK Dual Indenter Microhardness Tester

Technical Specifications - ALPHA-MHT-1000VK

Parameter Specification
Test Force Range 10gf to 1000gf
Optical Magnification 100X, 400X (10X and 40X objectives)
Indenter Types Vickers, Knoop
Dwell Time 0.95 seconds
Resolution 0.1µm
Construction Aluminum and stainless steel
Maximum Sample Height 3.5 inches (90 mm)
Dimensions (WxDxH) 17 x 19 x 17 inches (425 x 490 x 425 mm)
Weight 77 lbs (35 kg)
Part Number ALPHA-MHT-1000VK