Our polishing consumables ensure superior surface finishes for metallographic sample preparation. We offer pads and cloths for various materials, along with monocrystalline and polycrystalline diamond suspensions for precise polishing and minimal surface deformation, ensuring accurate microstructural analysis.
Tips
- Select the Right Pad - Soft cloths are best for final polishing; harder pads suit intermediate stages.
- Use Diamond Suspensions - Monocrystalline for aggressive polishing; polycrystalline for finer finishes.
- Prevent Contamination - Clean pads between steps to avoid cross-contamination.
- Magnetic System - Simplifies pad changes, improving workflow and reducing downtime.