Equipment / Abrasive Sectioning

MEGA Series Abrasive Cutting

PACE Technologies’ abrasive sectioning equipment delivers clean, precise cuts for metals, ceramics, and more. Manual and automated models support efficient sample prep while preserving microstructural integrity.

Manual Abrasive Cutters

Manual abrasive cutting provides precise control and flexibility, ideal for small batches and custom cuts. Operators can adjust feed rates and positioning, making it suitable for metals, ceramics, and composites. Its simplicity and lower costs make it a practical choice for highly customized applications.


Abrasive Cutting Equipment

MEGA-M250S Manual Abrasive Cutter

The MEGA-M250S is an economical manual 250mm wheel feed for hands-on control. It efficiently handles a variety of materials, providing versatile cutting capabilities.

  • Maximum Cut-Off Blade Diameter: 250 mm (~10 inches)
  • Cutting Capacity:
    • Diameter: Up to 2.5 inches (65 mm)
    • Height x Depth: 3 x 7 inches (75 x 175 mm)
  • Z-Axis Wheel Feed Range: 3.25 inches (82 mm)

The t-slotted stainless steel table, measuring 9.75 x 9 inches (250 x 230 mm), offers a stable platform for cutting. To maintain optimal performance, the MEGA-M250S includes a robust 14-gallon (53 liters) cooling unit. Its 3 hp (2.2 kW) asynchronous motor runs at variable speeds from 300 to 3000 rpm and is adaptable to cutting forces of 3-15 amps.

Abrasive Cutting Equipment

MEGA-T250S

The MEGA-T250S is designed for precision and versatility, featuring both manual wheel (250mm) and table feeds for enhanced control.

  • Maximum Cut-Off Blade Diameter: 250 mm (~10 inches)
  • Cutting Capacity:
    • Diameter: Up to 3 inches (75 mm)
    • Height x Depth: 2 x 8 inches (50 x 200 mm)
  • Z-Axis Wheel Feed Range: 3.9 inches (100 mm)
  • Y-Axis Table Feed Range: 3.3 inches (84 mm)

The spacious t-slotted stainless steel table, measuring 11 x 18.25 inches (280 x 470 mm), provides a stable and durable platform for precise cuts. The MEGA-T250S is built to deliver reliable performance in demanding applications, ensuring accuracy and efficiency in every operation.

Abrasive Cutting Equipment

MEGA-T300S

The MEGA-T300S offers reliable precision and control for various cutting applications using up to a 300mm wheel. It is designed for versatility and ease of use, featuring both manual wheel and table feeds.

  • Maximum Cut-Off Blade Diameter: 300 mm (~12 inches)
  • Cutting Capacity:
    • Diameter: Up to 4 inches (100 mm)
    • Height x Depth: 3 x 8 inches (75 x 200 mm)
  • Z-Axis Wheel Feed Range: 3.9 inches (100 mm)
  • Y-Axis Table Feed Range: 7 inches (175 mm)

The sturdy t-slotted stainless steel table, measuring 11 x 18.25 inches (280 x 470 mm), provides a stable platform for accurate cuts. The MEGA-T300S accommodates a wide range of cutting configurations, ensuring precise performance in demanding applications.

Abrasive Cutting Equipment

MEGA-T350S

The MEGA-T350S is standalone machine designed to provide reliable precision and control for various cutting applications. It features manual wheel (350mm) and table feeds for versatility and ease of use.

  • Maximum Cut-Off Blade Diameter: 350 mm (~14 inches)
  • Cutting Capacity:
    • Diameter: Up to 4.5 inches (115 mm)
    • Height x Depth: 3 x 6 inches (75 x 150 mm)
  • Z-Axis Wheel Feed Range: 3 inches (75 mm)
  • Y-Axis Table Feed Range: 5.9 inches (150 mm)

The sturdy t-slotted stainless steel table, measuring 28 x 16 inches (710 x 400 mm), provides a stable platform for accurate cuts. The MEGA-T350S accommodates a wide range of cutting configurations, ensuring precise performance in demanding applications.

Abrasive Cutting Equipment

MEGA-T400S

The MEGA-T400S is our most advanced manual abrasive cutting machine designed to meet the demands of abrasive cutting with its robust features and user-friendly interface. It is equipped with both manual wheel (400mm) and table feeds, including a touch screen for enhanced control and ease of operation.

  • Maximum Cut-Off Blade Diameter: 400 mm (~16 inches)
  • Cutting Capacity:
    • Diameter: Up to 6 inches (150 mm)
    • Height x Depth: 3 x 6 inches (70 x 150 mm)
  • Z-Axis Wheel Feed Range: 5 inches (125 mm)
  • Y-Axis Table Feed Range: 5.9 inches (150 mm)

The t-slotted stainless steel table, measuring 28 x 15.75 inches (710 x 400 mm), provides a stable and durable platform for accurate cuts. The MEGA-T400S offers flexibility for a variety of cutting configurations, ensuring precise performance in demanding applications.


Automated Abrasive Cutters

Automated abrasive cutting enhances your overall precision and efficiency, ideal for high throughput labs. With programmable controls, our machines ensure consistent cuts across materials while minimizing operator error. Their advanced features make them perfect for applications demanding precision, speed, and scalability.

Abrasive Cutting Equipment

MEGA-T300A

The MEGA-T300A Automated Cutter is our only table-top automated abrasive cutting machine. It combines precision and automation for efficient cutting applications. It features both automated and manual table feeds with a manual wheel feed (300mm), offering flexibility and control in various operations.

  • Maximum Cut-Off Blade Diameter: 300 mm (~12 inches)
  • Cutting Capacity:
    • Diameter: Up to 4 inches (100 mm)
    • Height x Depth: 3 x 8 inches (75 x 200 mm)
  • Z-Axis Wheel Feed Range: 3.9 inches (100 mm)
  • Y-Axis Table Feed: 7 inches (175 mm) with a feed rate of 0.04-0.20 inches/sec (0.1 - 5 mm/sec)
  • X-Axis Table Feed: 1.8 inches (45 mm) with a feed rate of 0.04-0.40 inches/sec (0.1 - 10 mm/sec)
  • Pulse Mode: 0.5-5A

The t-slotted stainless steel table, measuring 11 x 18.25 inches (280 x 470 mm), provides a stable platform for accurate cuts. The MEGA-T300A's automated and manual capabilities ensure precise performance in demanding applications, making it ideal for high-precision tasks.

Abrasive Cutting Equipment

MEGA-T350A

The MEGA-T350A is a standalone Automated Abrasive Cutter. It delivers precision and versatility for efficient cutting operations. It features both automated and manual table feeds combined with a manual wheel feed (350mm), providing flexible control for diverse applications.

  • Maximum Cut-Off Blade Diameter: 350 mm (~14 inches)
  • Cutting Capacity:
    • Diameter: Up to 4.5 inches (115 mm)
    • Height x Depth: 3 x 6 inches (75 x 150 mm)
  • Z-Axis Wheel Feed Range: 3 inches (75 mm)
  • Y-Axis Table Feed: 7 inches (175 mm) with a feed rate of 0.04-0.20 inches/sec (0.1 - 5 mm/sec)
  • X-Axis Table Feed: 1.8 inches (45 mm) with a feed rate of 0.04-0.40 inches/sec (0.1 - 10 mm/sec)
  • Pulse Mode: 0.5-5A

The t-slotted stainless steel table, measuring 11 x 18.25 inches (280 x 470 mm), provides a stable platform for precise cuts. The MEGA-T350A's advanced features ensure accurate performance in demanding environments, making it ideal for a wide range of cutting tasks.

Abrasive Cutting Equipment

MEGA-T400A

The MEGA-T400A is our most advanced Automated Abrasive Cutter. It combines advanced technology with user-friendly design to meet the demands of abrasive cutting. It features both automated and manual table feeds with a manual wheel feed (400mm) and includes a touch screen for enhanced control and ease of operation.

  • Maximum Cut-Off Blade Diameter: 400 mm (~16 inches)
  • Cutting Capacity:
    • Diameter: Up to 6 inches (150 mm)
    • Height x Depth: 3 x 6 inches (70 x 150 mm)
  • Z-Axis Wheel Feed Range: 5 inches (125 mm)
  • Y-Axis Table Feed: 5.9 inches (150 mm) with a feed rate of 0.04-0.20 inches/sec (0.1 - 5 mm/sec)
  • X-Axis Table Feed: 1.8 inches (45 mm) with a feed rate of 0.04-0.40 inches/sec (0.1 - 10 mm/sec)
  • Pulse Mode: 0.5-5A

The t-slotted stainless steel table, measuring 28 x 15.75 inches (710 x 400 mm), provides a stable and durable platform for precise cuts. The MEGA-T400A's touch screen interface and automated features ensure efficient and accurate performance for a variety of cutting tasks.