Equipment / Hardness Testers

Hardness Testing Equipment

PACE Technologies offers reliable hardness testers for metallographic applications, including Microhardness, Brinell, MacroVickers, and Rockwell models. These instruments deliver consistent performance with the essential features needed for accurate materials testing.

Microhardness Testers

Microhardness testers provide precise measurements for small or delicate materials, using minimal force to accurately assess coatings, films, and microstructures. Ideal for labs and quality control, they offer reliable Vickers and Knoop testing in one compact device.

Microhardness Tester ALPHA-MHT-1000Z

ALPHA-MHT-1000Z - Microhardness Tester

The ALPHA-MHT-1000Z microhardness tester is designed for accurate Vickers or Knoop hardness testing, ideal for small samples or thin coatings. It offers precise control with an auto turret and digital measurements.

  • Indenter Types: Vickers or Knoop
  • Objective Magnification: 10X and 40X
  • Testing Force: 10-1000 gf
  • Testing Range: 1 HV ~ 3000 HV
  • Dimensions (WxDxH): 13 x 19 x 22-inch
  • Weight: 88 lbs
Microhardness Tester ALPHA-MHT-2000Z2

ALPHA-MHT-2000Z2 - Microhardness Tester

The ALPHA-MHT-2000Z2 microhardness tester combines Vickers and Knoop testing with advanced digital features. It includes an auto turret, touch screen, and automatic hardness conversion for streamlined testing.

  • Indenter Types: Vickers or Knoop
  • Objective Magnification: 10X and 40X
  • Testing Force: 10-2000 gf
  • Testing Range: 1 HV ~ 3000 HV
  • Dimensions (WxDxH): 17 x 19 x 17-inch
  • Weight: 68 lbs
Automated Microhardness Tester ALPHA-AUTO-MHT

ALPHA-MHT-AUTO - Automated Microhardness Tester

The ALPHA-MHT-AUTO is an automated microhardness tester that simplifies the testing process with its auto-loading, dwell, and unloading features. It’s perfect for high-throughput environments requiring consistent, reliable results.

  • Indenter Types: Vickers or Knoop
  • Objective Magnification: 10X and 40X
  • Testing Force: 10-1000 gf
  • Testing Range: 1 HV ~ 3000 HV
  • Dimensions (WxDxH): 13.2 x 22 x 26.6-inch
  • Weight: 115 lbs
Dual Indenter Microhardness Tester ALPHA-MHT-1000VK

ALPHA-MHT-1000VK - Dual Indenter Microhardness Tester

The ALPHA-MHT-1000VK is a versatile dual indenter microhardness tester supporting both Vickers and Knoop tests. With auto turret, touch screen, and advanced features, it's designed for comprehensive microhardness testing.

  • Indenter Types: Vickers or Knoop
  • Objective Magnification: 10X, 20X, and 40X
  • Testing Force: 10-1000 gf
  • Testing Range: 1 HV ~ 3000 HV
  • Dimensions (WxDxH): 12 x 19.5 x 22-inch
  • Weight: 73 lbs

Rockwell Testers

Rockwell hardness testers deliver dependable and accurate hardness measurements across a range of materials. Designed for both manual and automated testing, these machines are perfect for diverse industrial applications, providing reliable results on a variety of Rockwell scales. With options for digital, semi-automated, and fully automated testing, they are well-suited for quality control in both production and laboratory settings.

Manual Rockwell Hardness Tester

OMEGA-RT - Manual Rockwell Hardness Tester

The OMEGA-RT is a cost-effective manual Rockwell hardness tester, ideal for basic testing needs. It supports key Rockwell scales and is manually controlled for precise hardness testing.

  • Rockwell Scales: HRA, HRB, HRC
  • Preliminary Test Force: 10 Kgf (98.07N)
  • Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
  • Loading Control: Manual
  • Instrument Throat Height: 6.5-inch (165 mm)
  • Dimensions (WxDxH): 7.2 x 21.5 x 29.7-inch
  • Weight: 200 lbs (90 kg)
Manual Rockwell Hardness Tester

OMEGA-RT2 - Manual Rockwell Hardness Tester

The OMEGA-RT2 offers the same reliable performance as the OMEGA-RT but with a slightly different footprint, making it a versatile option for basic manual Rockwell hardness testing.

  • Rockwell Scales: HRA, HRB, HRC
  • Preliminary Test Force: 10 Kgf (98.07N)
  • Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
  • Loading Control: Manual
  • Instrument Throat Height: 6.5-inch (165 mm)
  • Dimensions (WxDxH): 9.6 x 20.5 x 27.6-inch
  • Weight: 172 lbs (78 kg)
Digital Semi-Automated Rockwell Hardness Tester

OMEGA-DIGI-RT - Digital Semi-Automated Rockwell Hardness Tester

The OMEGA-DIGI-RT is a digital Rockwell hardness tester that provides semi-automated testing with digital precision. It supports a wide range of Rockwell scales and automatic hardness conversion.

  • Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
  • Preliminary Test Force: 10 Kgf (98.07N)
  • Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
  • Hardness Resolution: 0.1 HR
  • Dwell Time: Adjustable 1-60 seconds
  • Instrument Throat Height: 6.9-inch (175 mm)
  • Dimensions (WxDxH): 7 x 21.5 x 30-inch
  • Weight: 265 lbs (120 kg)
Digital Rockwell Hardness Tester

OMEGA-RT-60/150 - Digital Rockwell Hardness Tester

The OMEGA-RT-60/150 is a versatile digital Rockwell hardness tester designed for a variety of hardness scales and automated testing features, making it suitable for complex testing environments.

  • Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
  • Preliminary Test Force: 10 Kgf (98.07N)
  • Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
  • Hardness Resolution: 0.1 HR
  • Dwell Time: Adjustable 1-60 seconds
  • Instrument Throat Height: 6.3-inch (160 mm)
  • Dimensions (WxDxH): 8.5 x 20 x 28-inch
  • Weight: 200 lbs (90 kg)
Automated Rockwell Hardness Tester

OMEGA-AUTO-RT - Automated Rockwell Hardness Tester

The OMEGA-AUTO-RT offers fully automated Rockwell hardness testing, with a broad range of supported scales and precision measurement, ideal for high-throughput testing environments.

  • Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
  • Preliminary Test Force: 10 Kgf (98.07N)
  • Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
  • Hardness Resolution: 0.1 HR
  • Dwell Time: Adjustable 1-60 seconds
  • Instrument Throat Height: 11 inches (280 mm)
  • Dimensions (WxDxH): 9 x 24 x 34.8-inch
  • Weight: 265 lbs (120 kg)

Dual Rockwell / Superficial Testers

Dual Rockwell / Superficial hardness testers provide precise and consistent hardness measurements for a wide range of materials. Tailored for both Rockwell and Superficial Rockwell scales, these testers are ideal for versatile industrial applications. Whether you require manual, semi-automated, or fully automated solutions, these machines offer reliable performance for quality control in production environments and laboratory settings. With digital and automated options, they ensure accurate and efficient testing, making them essential tools for maintaining high standards in material testing.

Digital Dual Rockwell / Superficial Hardness Tester

OMEGA-SRT-15/150 - Digital Dual Rockwell / Superficial Hardness Tester

The OMEGA-SRT-15/150 is a versatile digital tester that offers both Rockwell and Superficial Rockwell hardness testing. With adjustable test forces and auto hardness conversion, it's ideal for a wide range of materials and applications.

  • Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV, HR15N, HR30N, HR45N, HR15T, HR30T, HR45T
  • Test Forces: 3 Kgr (Superficial), 10 Kgr (Rockwell)
  • Full Test Forces: 15, 30, 45 Kgf (Superficial); 60, 100, 150 Kgf (Rockwell)
  • Resolution: 0.1 HR
  • Instrument Throat Height: 6.3 inches (160 mm)
  • Dimensions (WxDxH): 7 x 21.5 x 30 inches (182 x 546 x 755 mm)
  • Weight: 200 lbs (90 kg)
Digital Semi-Automated Dual Rockwell / Superficial Hardness Tester

OMEGA-DIGI-RST - Digital Semi-Automated Dual Rockwell / Superficial Hardness Tester

The OMEGA-DIGI-RST combines digital precision with semi-automated operation, offering efficient dual Rockwell and Superficial Rockwell hardness testing. It includes auto hardness conversion and adjustable dwell time for consistent results.

  • Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
  • Test Forces: 3 Kgr (Superficial), 10 Kgr (Rockwell)
  • Full Test Forces: 15, 30, 45 Kgf (Superficial); 60, 100, 150 Kgf (Rockwell)
  • Resolution: 0.1 HR
  • Instrument Throat Height: 6.9 inches (175 mm)
  • Dimensions (WxDxH): 9 x 24 x 34.8 inches (225 x 615 x 885 mm)
  • Weight: 265 lbs (120 kg)
Automated Dual Rockwell / Superficial Hardness Tester

OMEGA-AUTO-RST - Automated Dual Rockwell / Superficial Hardness Tester

The OMEGA-AUTO-RST offers fully automated testing for both Rockwell and Superficial Rockwell scales. It features easy operation, precise control, and auto hardness conversion, making it a reliable tool for high-throughput testing environments.

  • Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
  • Test Forces: 3 Kgr (Superficial), 10 Kgr (Rockwell)
  • Full Test Forces: 15, 30, 45 Kgf (Superficial); 60, 100, 150 Kgf (Rockwell)
  • Resolution: 0.1 HR
  • Instrument Throat Height: 6.9 inches (175 mm)
  • Dimensions (WxDxH): 9 x 24 x 34.8 inches (225 x 615 x 885 mm)
  • Weight: 265 lbs (120 kg)

Brinell / MacroVickers Testers

Brinell and MacroVickers hardness testers are essential tools for evaluating the hardness of larger and bulkier specimens. These testers are designed to handle a wide range of test forces, making them versatile for various industrial applications. With options ranging from manual to fully automated systems, they provide reliable and consistent hardness measurements, ensuring quality control in both production and laboratory settings.

Digital Semi-Automated MacroVickers Hardness Tester

OMEGA-5000-VZ - Digital Semi-Automated MacroVickers Hardness Tester

The OMEGA-5000-VZ offers semi-automated precision in MacroVickers hardness testing. With a wide range of test forces and automatic shifting between objectives and indenters, it’s perfect for detailed metallographic analysis.

  • Test Forces: 1 kgf, 2 kgf, 2.5 kgf, 3 kgf, 5 kgf, 10 kgf, 20 kgf, 30 kgf, 50 kgf
  • Magnification: 100X, 200X
  • Loading Method: Automatic
  • Dwell Time: Adjustable 5-60 seconds
  • Max Sample Height: 6.7 inches (170 mm)
  • Dimensions (WxDxH): 11 x 21 x 25 inches (280 x 530 x 630 mm)
  • Weight: 77 lbs (35 kg)
Manual Brinell Hardness Tester

OMEGA-HB - Manual Brinell Hardness Tester

The OMEGA-HB is a straightforward manual Brinell tester, offering reliable performance at a low cost. Ideal for basic hardness testing needs, it’s equipped with a 20X optical scope for precise measurements.

  • Measuring Range: 3.2 to 650 HBW
  • Test Forces: 187.5, 250, 500, 750, 1000, 3000 kgf
  • Max Height of Specimen: 8.1 inches (205 mm)
  • Instrument Throat Height: 5.3 inches (135 mm)
  • Dimensions (WxDxH): 9.3 x 21.5 x 29.7 inches (235 x 545 x 755 mm)
  • Weight: 290 lbs (130 kg)
Digital Brinell Hardness Tester

OMEGA-HB-3000 - Digital Brinell Hardness Tester

The OMEGA-HB-3000 is a digital Brinell tester, designed for more advanced testing applications. It offers a wide range of test forces and digital precision, making it suitable for detailed hardness analysis in larger samples.

  • Test Forces: 62.5, 100, 125, 187.5, 250, 500, 750, 1000, 1500, 3000 kgf
  • Testing Range: ~8 to 650 HBW
  • Max Height of Specimen: 8.8 inches (225 mm)
  • Max Width of Specimen: 5.3 inches (135 mm)
  • Dimensions (WxDxH): 9.3 x 21.5 x 31.1 inches (235 x 545 x 790 mm)
  • Weight: 290 lbs (130 kg)
Fully Automated Digital Brinell Hardness Tester

OMEGA-AUTO-HB - Fully Automated Digital Brinell Hardness Tester

The OMEGA-AUTO-HB offers full automation in Brinell hardness testing, making it ideal for high-throughput environments. It features a range of test forces and can handle larger specimens, ensuring consistent and accurate results.

  • Test Forces: 62.5, 100, 125, 187.5, 250, 500, 750, 1000, 1500, 3000 kgf
  • Testing Range: ~8 to 650 HBW
  • Max Height of Specimen: 10 inches (260 mm)
  • Max Width of Specimen: 6 inches (150 mm)
  • Dimensions (WxDxH): 12 x 24.5 x 39 inches (313 x 622 x 992 mm)
  • Weight: 200 lbs (170 kg)