PACE Technologies' abrasive belts, rolls, and powders are designed to meet the rigorous demands of metallographic sample preparation. Available in silicon carbide, alumina, and diamond variants, these consumables provide flexible, high-efficiency material removal across metals, ceramics, and composites.
Abrasive Grinding Consumables
Abrasive belts, rolls, and powders from PACE Technologies offer versatile solutions for metallographic grinding across a wide range of materials. These silicon carbide (SiC)-based consumables provide sharp, fast-cutting performance ideal for routine material removal and surface conditioning. Rolls allow for custom sizes, belts are designed for automated systems, and powders are used with cloths or composite surfaces for maximum flexibility. Whether working with soft metals, ceramics, or composites, these abrasives are optimized to minimize surface deformation, improve workflow efficiency, and deliver reproducible results throughout the preparation process.
Material | Objective | Recommended SiC Product Format |
---|---|---|
Soft non-ferrous metals (Aluminum, Brass, Zinc) | Minimize embedding & deformation | P240–P1200 grit SiC Belts or Rolls |
Ferrous metals (Low carbon steel, Stainless steel) | Reduce deformation & prepare for polishing | P180–P600 grit SiC Belts or Rolls |
Tool steels, case-hardened alloys | Planarize & minimize work hardening | P120–P320 grit SiC Belts or Rolls |
Refractory metals (W, Mo, Ti) | Avoid smearing & surface damage | P320–P800 grit SiC Rolls or Loose Powder |
Ceramics & minerals | Remove surface defects with minimal chipping | 240–400 grit SiC Belts; or 15–30µm SiC Powder |
Composites (MMCs, PMCs) | Preserve matrix & minimize edge rounding | P240–P400 grit SiC Belts or Rolls |