PICO-200A Automatic Table Feed Saw
Item ID: PICO-200A
An automatic table-feed saw with 2-inch cutting capacity, laser alignment, and variable speed (500-3000 rpm). Built for precise, hands-off sectioning of a wide range of materials.
Features
- Up to 2-inch (50 mm) cutting capacity with automatic table feed
- Built-in laser alignment for precise sample positioning
- Continuously adjustable speed (500-3000 rpm)
- Integrated 5-liter coolant tank for effective heat management
Technical Specifications
| Parameter | Specification |
|---|---|
| Cut-off Blade Size | Max. diameter 200 mm (8 inches) |
| Cutting Capacity | 50 mm (2 inches) |
| Specimen Feed | Table feed |
| Coolant Tank | 5 Liters |
| Arbor Size | 12.7 mm (0.5-inch) |
| Variable Speed (RPM) | 500-3000 rpm continuously adjustable |
| Rated Power | 1100W |
| Electrical Specification | 110V or 220V (50/60 Hz) |
| Dimensions (WxDxH) | Closed: 22.4 x 28.3 x 16-inch (570 x 717 x 405mm) / Open: 22.4 x 28.3 x 35-inch (570 x 717 x 900mm) |
| Weight | 63 kg (139 lbs) |
| Catalog Number | PICO-200A |