Skip to main content

Compression Mounting Consumables

Our compression mounting consumables deliver reliable, efficient mounting for metallographic sample preparation. Choose from high-performance thermosetting and thermoplastic resins designed for strong adhesion, low shrinkage, and clear, reliable mounts. Engineered to preserve sample geometry, our products ensure accurate results for microstructural analysis.

Compression Mounting Consumables

Key Considerations

Choose the Right Resin

Match the resin type to material requirements for optimal edge retention and mounting quality.

Minimize Shrinkage

Select low-shrinkage compounds to preserve sample geometry and prevent mounting gaps.

Match Visibility Needs

Choose resins with suitable clarity and adhesion for inspection and reliable prep during grinding and polishing.

Introduction

Compression mounting is a very useful mounting technique which can provide better specimen edge retention compared to castable mounting resins. Compression mounting resins are available in different colors and with various fillers to improve hardness or conductivity.

Several compression mounting characteristics include:

  • Convenient means to hold the specimen
  • Provides a standard format to mount multiple specimens
  • Protects edges
  • Provides proper specimen orientation
  • Provides the ability to label and store the specimens
TERAPRESS metallographic compression mounting press

Compression mounts are quick and easy to produce, requiring several minutes to cure at the appropriate mounting temperature. Most of the time required in compression mounting occurs during the heating and cooling cycles. When choosing a compression mounting machine, the most important features include its maximum heating temperature and how intimately the heater and water cooler are connected to the mold assembly. The better compression mounting machines have heaters which can reach temperatures of at least 200°C (450°F). For faster turn around time, water cooling is essential.

Mounting Resin Properties

There are a variety of compression mounting materials. The two main classes of compression mounting materials are thermoset and thermoplastics. Thermoset resins require heat and pressure to cross-link the polymer and the reaction is irreversible. Thermoplastic, on the other hand, can theoretically be remelted.

Phenolics Acrylics Epoxy (Glass-Filled) Diallyl Phthalates
Cost Low Moderate Moderate Moderate
Ease of use Excellent Moderate Good Good
Availability of colors Yes No No Yes
Cycle times Excellent Moderate Good Good
Edge retention Fair Good Excellent Excellent
Clarity None Excellent None None
Hardness Low Medium High High

TIP: Compression mounting at higher than the recommended minimum temperature generally improves the properties of the mount.

TIP: A useful tip for marking or identifying a specimen is to mold the label inside of the mount. If the entire mount is an acrylic, just place the label on top the mount and cover it with a little acrylic powder. To label other compression mounting resins, add a thin layer of acrylic over the other mounting material and then position the label on this layer. Finish off the mount with another layer of acrylic.

Acrylic mount labeling example

Products

Phenolic Resins

View collection →

In general, phenolics are used because of their relatively low cost. In addition, phenolics are available in a variety of colors.

TIP: Use different color phenolics to color code jobs, specimens types, or for different testing dates. For example, changing the phenolic color each month will show which samples or jobs are getting old.

TIP: If the color dye in the mount bleeds out when rinsing with an alcohol, this is an indication that the mount was not cured either at a high enough temperature or for the proper length of time.

Description Quantity Catalog Number Image
Phenolic powder - Black 5 lbs (2.3 kg)
25 lbs (11.4 kg)
CM-2001B-5
CM-2001B-25
Black phenolic powder
Phenolic powder - Red 5 lbs (2.3 kg)
25 lbs (11.4 kg)
CM-2001R-5
CM-2001R-25
Red phenolic powder
Phenolic powder - Green 5 lbs (2.3 kg)
25 lbs (11.4 kg)
CM-2001G-5
CM-2001G-25
Green phenolic powder (placeholder)
Phenolic powder - Orange 5 lbs (2.3 kg)
25 lbs (11.4 kg)
CM-2001OR-5
CM-2001OR-25
Orange phenolic powder (placeholder)
Phenolic powder - White 5 lbs (2.3 kg)
25 lbs (11.4 kg)
CM-2001W-5
CM-2001W-25
White phenolic powder

Acrylic Resins

View collection →

The main application for compression mounting acrylics is based on their excellent clarity. This is particularly important for locating a specific feature within the specimen mount.

TIP: A common problem, known as the "cotton ball" effect, can occur with thermoplastic resins if they are heated to too high a temperature too fast so a liquid layer forms around the unmelted resin giving it the appearance of a cotton ball in the middle of the mount. To avoid this problem mount at a lower temperature (120-140°C), however, to correct this problem after the fact, simply put the mount back into the mounting press and either increase the time. Eventually this will eliminate the "cotton ball."

Description Quantity Catalog Number Image
Transacrylic Resin Powder (Transparent) 5 lbs (2.3 kg)
25 lbs (11.4 kg)
CM-2101A-5
CM-2101A-25
Acrylic resin powder

Epoxy Resins

View collection →

Glass-filled epoxies and diallyl phthalates are compression mounting resins used to provide a harder mounting support edge next to the specimen. These resins are commonly used to support the edges of coatings, heat treated samples and other specimens requiring better flatness.

TIP: Epoxies (glass-filled) and diallyl phthalates are significantly more expensive than phenolic and acrylics. In order to reduce the cost of these mounts, they can be laminated with a lower cost mounting compound such as a phenolic. The technique is to place a sufficiently thick enough layer of the glass-filled epoxy or diallyl phthalate around the specimen in order to compensate for any grinding loss. The rest of the mount can then be supported with a lower cost compression mounting compound such as a phenolic. Red phenolics are used frequently for this technique.

Description Quantity Catalog Number Image
Epocomp Epoxy Resin Powder 5 lbs (2.3 kg)
25 lbs (11.4 kg)
EP-2201A-5
EP-2201A-25
Epoxy resin
Epocomp Epoxy FINE Resin Powder 5 lbs (2.3 kg)
25 lbs (11.4 kg)
EPF-2201A-5
EPF-2201A-25
Epoxy resin

Diallyl Phthalate Resins

View collection →

Diallyl phthalate resins provide excellent edge retention and are particularly suitable for hard materials and specimens requiring precise edge preservation.

Description Quantity Catalog Number Image
Diallyl Phthalate Compression Resin Powder (Short-Glass Filled) 5 lbs (2.3 kg)
25 lbs (11.4 kg)
DY-2301A-5
DY-2301A-25
Diallyl Phthalate Resin

Conductive Resins

View collection →

With the addition of fillers such as graphite or copper, the compression mounting compounds can be made conductive. Conductive mounts are used in scanning electron microscopes (SEM) to prevent the specimen from building up a charge. Conductive mounts are also used for specimens requiring electrolytic etching or polishing.

Description Quantity Catalog Number Image
Conductive (Graphite) Resin Powder 2.5 lbs (1.1 kg)
5 lbs (2.3 kg)
CONDUCTO-1
CONDUCTO-5
Conductive Graphite Resin

Miscellaneous Accessories

Description Quantity Catalog Number Image
30 ml Measuring Scoop 30 ml MS-1000-30 Measuring Scoop
Mold Release 8 oz (237 ml)
16 oz (473 ml)
MR-1000-08
MR-1000-16
Mold Release

Recommended Compression Mounting Procedures

  • Clean specimens to remove cutting and handling residues
  • Remove debris from mold assembly
  • Apply thin coat of mold release compound to mold assembly
  • Raise mold ram to up position
  • Center specimen on ram
  • Lower ram assembly
  • Pour predetermined amount of resin into mold
  • Clean and remove any excess resin from around the mold assembly threads
  • Lock mold assembly cover
  • Slowly raise ram into up position
  • Apply recommended heat and maintain pressure for specified period of time
  • Cool to near room temperature
  • Remove mounted specimen
  • Clean mold and ram assembly

TIP: Preheat resin and sample to 35°C (95°F) to expedite the initial heating process and for increasing throughput.

Troubleshooting

Symptom Cause Solution
Large bubbles in acrylic resins Curing temperature too high or mounting press has insufficient mounting pressure Reduce temperature (120-140°C) and increase mounting pressure
Soft surfaces on mount Mount did not completely polymerize because of polymer incompatibility with mold release or oil on the specimen surface Clean specimen and mounting machine to remove incompatible coatings. Use a compatible mold release
Voids or cracks High internal stress due to overly rapid cooling Allow mounts to cool more slowly and longer
Haze around specimen (acrylic mounts) Specimen contains moisture or contains copper or some other polymerization retarding alloy Use a desiccator or low temperature oven to dry specimen. Coat specimens with an appropriate lacquer before mounting
Phenolic dye leaching out with alcohol rinsing Insufficient mounting temperature Increase mounting temperature or service check heater element
Distortion or cracking of specimen Autoclave pressure is too great for the specimen Reduce mounting pressure or use a castable epoxy resin

Related Equipment

TP-7100S Pneumatic Mounting Press

TP-7100S

Pneumatic compression mounting press with automatic operation and precise temperature control. Features quick-release bayonet closure, digital display, and consistent pressure application for reliable, repeatable mounts.

TP-7500S Hydraulic Mounting Press

TP-7500S

Heavy-duty hydraulic mounting press delivering up to 75kN force for demanding applications. Features programmable cycles, advanced safety systems, and rugged construction ideal for high-volume production environments.

TP-Tank Recirculating Cooling System

TP-Tank

Recirculating water cooling system for compression mounting presses. Maintains optimal cooling rates, reduces water consumption, and ensures consistent mount quality with integrated temperature monitoring.

Frequently Asked Questions

Common questions about compression mounting

What is the difference between compression and castable mounting?

Compression mounting uses heat and pressure to cure thermosetting resins quickly (5-10 minutes), providing excellent edge retention and minimal shrinkage. Castable mounting uses room temperature or low-heat curing epoxy or acrylic resins, ideal for heat-sensitive samples. Compression mounting is faster and provides better edge retention, while castable mounting is gentler on delicate specimens and can encapsulate irregular shapes more easily.

How do I select the right compression mounting resin?

Resin selection depends on your application: Phenolic resins offer excellent edge retention and hardness for general metallography. Acrylic (transparent) resins allow optical examination of mounted samples. Epoxy resins provide superior adhesion and minimal shrinkage for critical applications. Diallyl phthalate resins offer excellent electrical insulation. Conductive resins are essential for SEM analysis. Consider sample material, analysis requirements, and whether you need electrical conductivity or transparency.

What temperature and pressure should I use for compression mounting?

Typical compression mounting conditions are 300-350°F (150-175°C) at 3,000-4,000 PSI for 5-10 minutes. However, exact parameters vary by resin type and sample material. Always consult the resin manufacturer's recommendations. Heat-sensitive samples may require lower temperatures or alternative mounting methods. Use a mounting press with precise temperature and pressure controls to ensure consistent results and avoid sample damage.

How can I prevent voids and incomplete mounting?

To prevent voids: 1) Ensure specimens are clean and dry before mounting, 2) Use adequate resin powder to completely surround the sample, 3) Apply proper pressure (3,000-4,000 PSI) throughout the curing cycle, 4) Maintain consistent temperature, 5) Allow sufficient curing time (typically 5-10 minutes), 6) Avoid rapid temperature changes, and 7) For porous materials, consider vacuum impregnation before mounting. Proper specimen placement and using release agents can also improve results.

Why is my mounted sample cracking or showing poor edge retention?

Cracking and poor edge retention typically result from: excessive mounting pressure (causing sample deformation), thermal shock (cooling too quickly), incompatible resin/sample thermal expansion, or insufficient curing time. To improve edge retention: use appropriate pressure for your sample type, allow gradual cooling, select resin with compatible thermal properties, ensure complete curing, and avoid excessive grinding pressure during preparation. For brittle materials, consider using filled resins or epoxy-based systems.

Can I reuse compression mounting molds and accessories?

Yes! Compression mounting molds, rams, and base plates are designed for thousands of uses. Clean them after each mounting cycle to prevent resin buildup and contamination. Use appropriate release agents (like MOLDRELEASE) to prevent sticking and extend mold life. Inspect molds regularly for wear, cracks, or damage. Replace release paper/film between each mount. Proper maintenance ensures consistent mount quality and extends equipment lifespan significantly.