Diamond is the hardest known material and makes a great grinding abrasive for many hard materials. The advantages and disadvantages of grinding with diamond are as follows:

Advantages:

  • Long lasting (most materials)
  • Hard and tough abrasive
  • Can be used for fixed, semi-fixed, and free abrasive applications

Disadvantages:

  • Does not work well with high carbon or hardened steels (diamond dulls due to reaction with ferrite structure)
  • Needs to be conditioned or dressed for optimum operation
  • Expensive

Metal vs. Resin Bond

There are two types of bonding for diamond grinding disks: metal and resin. Metal bonded diamond grinding disks are more aggressive and can produce more damage. Resin bonded disks will break down easier to produce a better surace finish, however, they typically have lower life.

Diamond / Composite Grinding Disks
Metallographic Diamond Grinding Disks



Current Selection
The following information is generated automatically for display only. Tax may be changed.

Total value ($) Choose Tax rate(%) Sub total ($)