Metallographic Phenolic Compression Mounting Powders
Phenolic Compression
Mounting Powders
2 / 5
Metallographic Glass Filled Mounting Powders for Edge Retention (Epoxy and Diallyl Phthalate) Powders
Glass Filled Mounting Powders
for Edge Retention (Epoxy and Diallyl Phthalate)
3 / 5
Metallographic Clear Thermoplastic Acrylic Powders
TRANSACRYLIC Clear
Mounting Powder
4 / 5
Metallographic conductive copper or graphite compression mounting powders
Conductive Mounting Powders
(with Copper or Graphite fillers)
5 / 5
Metallographic Compression Mounting Accessories and Miscellaneous
Compression Mounting
Accessories and Miscellaneous

Compression Mounting Characteristics

There are a variety of compression mounting materials. The two main classes of compression mounting materials are thermoset and thermoplastics. Thermoset resins require heat and pressure to cross-link the polymer, and the reaction is irreversible. Thermoplastic, on the other hand, can theoretically be remelted.

See the table below for more specific information on the various compression mounting resins: