PACE Technologies Banner logo



Click here to get a quote

Metallographic TERAPRESS TP-7100S Compression Mounting Press Video

TERAPRESS-7100S
Compression Mounting Press

Metallographic compression mounting presses TERAPRESS TP-7100S Compression Mounting Press
Click here to get a quote

Metallographic TERAPRESS TP-7100S Compression Mounting Press Specifications

Feature Specification
Mount size 1 to 2-inch (25-50 mm)
Force Pneumatic
Mold Cylinders Single Fixed or Interchangeable Sizes
Incoming pressure range Max. 95 psi
Maximum pressure 1450 psi
Heater Specification 1000 Watts (110V 15 amp)
2000 Watts (110V 20 amp)
2000 Watts (220V 10 amp)
Thermostat range Max 392°F (200°C)
Cooling System Water
Cooling control Manual, temperature, time
Electrical Specifications 110V or 220V
50/60 Hz
Dimensions
(W x D x H)
31 x 19 x 19-inch
(534 x 485 x 485 mm)
Weight 69 lbs (32 kg)
Recirculating / Coolant Tank (14 gal) with pump (optional) TP-TANK
TP-7100S molds TP-7100S molds

Return to top

Copyright 2006-2024
PACE TECHNOLOGIES® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved

PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies LinkIn PACE Technologies YouTube Videos