Description:

Iron and steels play an important role in the world of structural and mechancial metals. Steel, in particular, is very useful because its hardness, wearability and toughness can be altered significantly by heat treating and annealing processes. Steels can be classified into three categories for micrstrutural analysis based on their hardness.

Preparation Challenge:

Not particularly difficult to prepare, however when using SiC abrasive papers the sample must track over the entire diameter of the SiC paper to avoid uneven break down and thus creating uneven grinding across the mount.

Examples:
HARDENED STEEL PROCEDURES
High Carbon Steel (1095)
Metallographic micrograph for fast cooled high carbon steel

Manganese Vanadium Tool Steel
Metallographic micrograph of Manganese vanadium tool steel


Copyright 2006-2024
PACE TECHNOLOGIES® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved

PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies LinkIn PACE Technologies YouTube Videos