Description:

Cast Irons and White Irons are used for many applications. The reliabiity of cast iron depends on the microstructure of the graphite in the material. If the graphite forms flakes, then the cast iron will be brittle, becoming more so over time. Cast iron with the addition of either magnesium or cerium, results in the graphite forming nodules. Nodular cast iron has much better ductility than gray cast iron. White cast irons are manufactured by chilling the surface of the cast mold in order to prevent the formation of graphite during solidification.

Preparation Challenge:

Cast Irons are difficult materials to prepare properly because the graphite nodules or the graphite flakes are easily fractured and pulled out during preparation. By minimizing the sectioning damage and starting with a modest grit size SiC paper, retaining these difficult particles can be accomplished.

Examples:
IRON PROCEDURES
Cast Irons
Metallographic Cast Iron Nodules

White Metal
Metallographic white iron


Copyright 2006-2024
PACE TECHNOLOGIES® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved

PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies LinkIn PACE Technologies YouTube Videos