Ceramic Matrix Composites (CMC's)
Specimen Preparation (Class 10 Procedures)
Metallographic Class 10 sample preparation

Description:

Ceramic matrix composites are used for either their high temperature resistance or there low wear characteristics.

Preparation Challenge:

Specimen preparation of these materials requires that the brittle phases be maintained.

Examples:
CERAMIC MATRIX COMPOSITE PROCEDURES
SiC fiber - Silicon Nitride Matrix
SiC fibers in Si3N4 matrix

Hafnium Diboride in a Boron Nitride Matrix
HfB2 fibers in BN matrix

SiC particles - Silicon Nitride Matrix
SiC particles in Si3N4 matrix

SiC particles - Zirconium Diboride Matrix
Metallographic micrograph of SiC Zirconium Diboride ceramic matric composite


Copyright 2006-2024
PACE TECHNOLOGIES® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved

PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies LinkIn PACE Technologies YouTube Videos