Titanium Metallographic Procedures

Metallographic etchant database

Titanium and Titanium Alloys

Description:
Titanium and titanium alloys are excellent light weight, high strength materials with uses ranging from sunglass and glass frames to military fighter jets.

Preparation Challenge:
Titanium and titanium alloy specimen preparation is relatively straight forward and very similar to iron and steel preparation techniques.

Metallographic micrograph of titanium alloy
Metallographic micrograph of titanium alloy
Metallographic micrograph of cast titanium
Metallographic micrograph of wrought titanium
About Us | Site Map | Web Disclaimer | Terms and Conditions | Contact Us
Copyright © 2006-2017
PACE Technologies ® - 3601 E. 34th St. - Tucson, AZ 85713 USA
Telephone +1 520-882-6598 FAX +1 520-882-6599.
All Rights Reserved.


PACE Technologies facebook link   Blog us on Tumblr   Blog us on Tumblr   PACE Technologies Google+   PACE Technologies Google+   PACE Technologies Google+