Nickel and Super Alloys

Description:
Nickel and nickel superalloys are used mostly for there corrosion and temperature resiliency.

Preparation Challenge:
These materials can have a range of properties and following standard metallographic procedures generally produces the required results

 
Metallographic microstructure of Nimonic 90