Metallographic Procedures for Glass

Glass and Minerals

Description:
Glasses and minerals are generally fairly hard and have a tendency to fracture.

Preparation Challenge:
Proper specimen preparation requires that the damage during specimen preparation be minimized, even as early as the sectioning or cutting operation.

Metallographic microstructure of alumino-silicate glass
Metallographic microstructure of slag
Metallographic microstructure of graphite
Metallographic micrograph of Periclase
Metallographic micrograph of chalcopyrite
About Us | Site Map | Web Disclaimer | Terms and Conditions | Contact Us
Copyright © 2006-2017
PACE Technologies ® - 3601 E. 34th St. - Tucson, AZ 85713 USA
Telephone +1 520-882-6598 FAX +1 520-882-6599.
All Rights Reserved.


PACE Technologies facebook link   Blog us on Tumblr   Blog us on Tumblr   PACE Technologies Google+   PACE Technologies Google+   PACE Technologies Google+