Ceramic Matrix Composites (CMC's)

Description:
Ceramic matrix composites are used for either their high temperature resistance or there low wear characteristics.

Preparation Challenge:
Specimen preparation of these materials requires that the brittle phases be maintained.

SiC fibers in Si3N4 matrix
HfB2 fibers in BN matrix
SiC particles in Si3N4 matrix
Metallographic micrograph of SiC Zirconium Diboride ceramic matric composite
About Us | Site Map | Web Disclaimer | Terms and Conditions | Contact Us
Copyright © 2006-2017
PACE Technologies ® - 3601 E. 34th St. - Tucson, AZ 85713 USA
Telephone +1 520-882-6598 FAX +1 520-882-6599.
All Rights Reserved.


PACE Technologies facebook link   Blog us on Tumblr   Blog us on Tumblr   PACE Technologies Google+   PACE Technologies Google+   PACE Technologies Google+