Metallographic Castable Vacuum Mounting

Click here to get a quote

CASTABLE Vacuum Mounting

Vacuum mounting of castable mounting resins significantly improves penetration of voids and provides better edge retention. The LSSA-011 vacuum impregnation unit (Part No. LSSA-011) allows for pouring the resin under maximum vacuum and for mounting multiple specimens.

 

Metallographic compression mounting pressesVacuum mounting chamber Click here to get a quote

Feature

Specification

Bell jar

Tilting, retractable pouring arm

Mount size

1 to 2-inch diameter (25-50 mm)

Vacuum

Vacuum pump (sold separately)

Dimensions
(W x D x H)

12 x 12 x 12-inch
(300x 300 x 300 mm)

Weight 2.2 lbs (1 kg)

Return to top


Vacuum Pumps

Description

110V Vacuum Pump

220V Vacuum Pump

Flow Rate

2.5 CFM

7.2 m3/h

Ultimate Vacuum

10 Pa

0.2 Pa

Power

120 W -0.17 hp

370 W - 0.5 hp

Inlet Port

SAE and ACME ports

7/16-inch - 20

Dimensions (W x D x H) 11 x 4.75 x 9-inch
(279 x 120 x 229 mm)
13 x 5.5 x 10-inch
(337 x 138 x 254 mm)
Weight 16.5 lbs (7.5 kg) 22 lbs (10 kg)
Part No. VAC-110 VAC-220
Click here to get a quote

Return to top


Copyright © 2006-2017
PACE Technologies ® - 3601 E. 34th St. - Tucson, AZ 85713 USA
Telephone +1 520-882-6598 FAX +1 520-882-6599.
All Rights Reserved.


PACE Technologies facebook link   Blog us on Tumblr   Blog us on Tumblr   PACE Technologies Google+   PACE Technologies Google+   PACE Technologies Google+