Metallographic Laboratory Precision Saws

Click here to get a quote
Metallographic medium speed precision wafering saw Metallographic medium speed precision wafering saw Metallographic table feed precision wafering saw
Wafering Saws PICO 155 / PICO 155P PICO 175 PICO 200
Blade size 3-6 inch (75-150 mm) 3-7 inch (75 -175 mm) 8-inch (200 mm)
Cutting Capacity (max.) 2-inch (50 mm) 2.4-inch (60 mm), 4-inch (100 mm) with specimen rotation 1.5-inches (38 mm)
Coolant Gravity / Pump Auto Gravity
Variable Speed (rpm) 50-1500 rpm 50-5000 rpm 300-3000 rpm
Fixtures PICO 155 fixtures PICO 175 fixtures PICO 200 fixtures
Part No. PICO 155P PICO 175 PICO 200


PICO 155 Low to Medium Speed Precision Cutter gravity feed coolant

 

PICO 155 Description Specification
Cutting capacity Max diameter 2-inch (50 mm)
Coolant Gravity drag
Cut-off blade size 3-inch (75 mm) - 7-inch (175 mm)
Arbor size 0.5-inch (12.7 mm)
Variable Speed (rpm) 50-1500 rpm continuously adjustable with LED speed display
Cutting Load 0-1500 gram load
Micrometer feed distance 0 to 1-inch (0-25 mm)
Micrometer accuracy 2 microns
Motor power 125W (24V)
Electrical Specification 110V/220V (50/60 Hz) (single phase)
Dimensions
(W x D x H)

Hood closed: 19.5 x 22.5 x 15-inch
(495 x 570 x 375 mm)

Hood open 19.5 x 22.5 x 21-inch
(495 x 570 x 540 mm)

Weight 66 lbs (30 kg)
PICO 155 fixtures PICO 155 fixtures
Medium speed precision wafering saw

 

Metallographic medium speed precision wafering saw Click here to get a quote
 
 

PICO 155P Low to Medium Speed Precision Cutter with coolant pump (Part Number PICO-155P)

 

PICO 155P Description Specification
Cutting capacity Max diameter 2-inch (50 mm)
Coolant Dual nozzle with pump
Cut-off blade size 3-inch (75 mm) - 7-inch (175 mm)
Arbor size 0.5-inch (12.7 mm)
Variable Speed (rpm) 50-1500 rpm continuously adjustable with LED speed display
Cutting Load 0-1500 gram load
Micrometer feed distance 0 to 1-inch (0-25 mm)
Micrometer accuracy 2 microns
Motor power 125W (24V)
Electrical Specification 110V/220V (50/60 Hz) (single phase)
Dimensions
(W x D x H)

Hood closed:19 x 23 x 14.5-inch
(480 x 580 x 368 mm)

Hood open: 19 x 29 x 19-inch
(480 x 740 x 370 mm)

Weight 66 lbs (30 kg)
PICO 155P fixtures PICO 155P fixtures
Medium speed precision wafering saw

 

Metallographic medium speed precision wafering saw Click here to get a quote
 
 

PICO 175 High Speed Precision Cutter with coolant pump (Part Number PICO-175)

 

PICO 175 Cutter Description Specification
Cutting capacity 3-inches (75 mm)
Cut-off blade size Min 3-inch (75 mm)
Max 8-inch (200 mm)
Arbor size 0.5-inch (12.7 mm)
Travel Distances X-direction: 0-2.6 inches( 0-66 mm)
Y-direction: 0-3.4 (0-86mm)
Variable Speed (rpm) 50-5000 rpm continuously adjustable
Feed Rate 0.0024-7.1 inches/minute (0.01-3 mm/second)
Cutting Load 5-20 N (1-4.5 lbf)
Micrometer feed distance 0 to 4-inch (0-100 mm)
Micrometer accuracy 0.1 mm
Motor power 1.0 hp (750 W)
Electrical Specification 110V or 220V (50/60 Hz) (single phase)
Dimensions
(W x D x H)

Hood closed: 25 x 22.4 x 17.8-inch
(635 x 570 x 450-mm)

Hood open: 25 x 23 x 29-inch
(635 x 585 x 740 mm)

Weight 160 lbs (35 kg)
PICO 175 fixtures PICO 175 fixtures
High speed precision wafering saw

 

Metallographic medium speed precision wafering saw Click here to get a quote
 
 

PICO 155/175 Fixtures and Accessories

Description Part Number PICO 155/155P PICO 175 Image
Universal specimen vise P150-702 x x PICO 155 universal holder
Large single saddle vise with lip P150-702b x x PICO 155 Large single saddle vise with lip
Sample holder with double parallel vise for long specimens P150-703 x x PICO 155 Sample holder wit double parallel vise for long specimens
Sample holder for round and mounted specimens (1.25-inch) P150-707 x x PICO 155 Sample holder for round and mounted specimens
Teardrop holder (18-40 mm)(0.7-1.6-inch) P150-710 x x PICO 155 Teardrop holder
Specimen vise for irregular shaped specimens P150-706 x x PICO 155 Specimen vise for irregular shaped specimens
Specimen vise for adhering specimens P150-709 x x PICO 155 Specimen vise for adhering specimens
Swivel arm unit for angular cutting P150-705 x PICO 155 Swivel arm unit for angular cutting
Fastener vise for longitudinal sectioning for fasteners, tubes etc. P150-711 x x PICO 155 Fastener vise for longitudinal sectioning for fasteners, tubes etc
50 mm diameter flanges P150-306 x x PICO 155 50 mm diameter flanges
75 mm diameter flanges P150-712 x x PICO 155 75 mm diameter flanges
Cutting table attachment for manual cutting of printed circuit board specimens P150-601 x n.a PICO 155 Cutting table attachment for manual cutting of printed circuit board specimens
Wafering blade dressing fixture, PICO 155 saws P150-701 x n.a PICO 155 Wafering blade dressing fixture
Wafering blade dressing fixture, PICO 175 saw P175-DF n.a x PICO 155 Wafering blade dressing fixture
Dovetail adapter for PICO 175 P175-750 n.a. x PICO 175 dove tail adapter
Locking blade rod for PICO 175 P175-755 n.a x PICO 175 locking handle

Return to top



The PICO 200 Variable Speed Table Saw (Part No. PICO-200)

 

PICO 200 Description Specification
Cutting capacity 1.5-inches (38 mm)
Specimen feed Table feed
Coolant tank 3 Liters
Cut-off blade size 8-inch (200 mm)
Arbor size 0.5-inch
Variable Speed (rpm) 300-3000 rpm continuously adjustable with LED speed display
Motor power 1.0 hp (750 W)
Electrical Specification 110V/220V (50/60 Hz) (single phase)
Dimensions
(W x D x H)
18 x 20 x 13.8-inch
(460 x 500 x 350 mm)
Weight 93 lbs (42 kg)
PICO 200 fixtures PICO 200 fixtures
Table feed precision wafering saw

 

Metallographic medium speed precision wafering saw Click here to get a quote
 
 

PICO 200 Fixtures and Accessories

PICO 200 Fixtures Part No.
Vertical clamping vise with shoe P200-V
Height adapter for P200-V vertical clamping vises P200-H
Angle cutting guide P200-ANGLE
Vacuum cleaning attachment P200-VAC

Return to top


About Us | Site Map | Web Disclaimer | Terms and Conditions | Contact Us

Copyright 2006-2017
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved


PACE Technologies facebook link   Blog us on Tumblr   Blog us on Tumblr   PACE Technologies Google+   PACE Technologies Google+   PACE Technologies Google+